Título: Column flotation of high grade fluorite without wash water addition
Título(s) alternativo(s): Mineral Processing and Extractive Metallurgy
Autor(es): Aliaga, Washington
Sampaio, C. H.
Brum, Irineu Antônio Schadach de
Ferreira, K. R. S.
Batistella, Marcos Antonio
Autor(es): Aliaga, Washington
Sampaio, C. H.
Brum, Irineu Antônio Schadach de
Ferreira, K. R. S.
Batistella, Marcos Antonio
Abstract: The present paper presents the results of fluorite flotation carried out on a column cell without wash water addition. Concentrate flow was obtained by making tailing flows smaller than feed flows. Hence, part of the feed water was carried up within bubble wakes. No pulp/froth interface was established. A high recovery was obtained in a 2 m collection zone column. The recovery reached >80% with a grade of ∼90%. It was found that the recovery depended on the value of the difference between the feed flow and tailing flow. In addition, a straight line between the surface velocity of mineral and the recovery was found. It appears that a maximum capacity of solid is ∼10 g min−1 cm−2.
Palavras-chave: Flotation
Fluorite
Tipo de Acesso: Acesso Aberto
URI: http://repositorio.ufba.br/ri/handle/ri/14384
Data do documento: 2007
Aparece nas coleções:Artigo Publicado em Periódico (PPEQ)

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
174328507X198654.pdf256 kBAdobe PDFVisualizar/Abrir


Os itens no repositório estão protegidos por copyright, com todos os direitos reservados, salvo quando é indicado o contrário.